[1]張忠鏵,董曉明.頁巖氣井套管變形原因分析及選材設計[J].石油管材與儀器,2020,6(04):24-29.[doi:10.19459/j.cnki.61-1500/te.2020.04.004]
 ZHANG Zhonghua,DONG Xiaoming.Deformation Analysis and Material Design of Production Casing for Shale Gas Well[J].Petroleum Tubular Goods & Instruments,2020,6(04):24-29.[doi:10.19459/j.cnki.61-1500/te.2020.04.004]
點擊復制

頁巖氣井套管變形原因分析及選材設計
分享到:

《石油管材與儀器》[ISSN:2096-0077/CN:61-1500/TE]

卷:
6
期數:
2020年04期
頁碼:
24-29
欄目:
頁巖氣專題
出版日期:
2020-08-20

文章信息/Info

Title:
Deformation Analysis and Material Design of Production Casing for Shale Gas Well
文章編號:
2096-0077(2020)04--0024-05
作者:
張忠鏵董曉明
寶山鋼鐵股份有限公司中央研究院 上海 201900
Author(s):
ZHANG Zhonghua DONG Xiaoming
Baosteel Central Research Institute, Baoshan Iron and Steel Co., Shanghai 201900, China
關鍵詞:
頁巖氣套管變形失效分析選材設計抗擠性能
Keywords:
shale gascasing deformationfailure analysis material design and selection anticollapse property
分類號:
TE931.2
DOI:
10.19459/j.cnki.61-1500/te.2020.04.004
文獻標志碼:
A
摘要:
針對川渝地區頁巖氣井生產套管出現的套變問題,采用理論計算和實物試驗相結合的方式,研究了生產套管在下入、固井、壓裂等服役條件下套管抗擠毀性能的變化規律并提出選材建議。結果表明,體積壓裂造成的井筒溫度降低、固井質量差以及套管受到地層應力導致的管體橢圓度增大均能明顯降低套管的抗擠毀性能。為改善套變問題,需要優化水平段套管設計,進一步提升套管的抗擠毀性能。
Abstract:
Aiming at the problem of production casing deformation in SichuanChongqing area, the variation of collapse property is studied by full scale test and theoretical calculation basing on the shale gas exploitation characteristics and the working conditions of production casing during tripping, cementing and fracturing process. The results show that the collapse property significantly declines under the influence of temperature changes of wellbore during fracturing, poor quality of well cementing and increased casing ovality due to wellbore pressure. In order to improve the problem of production casing deformation, it is necessary to enhance the anticollapse property by optimizing the material design of horizontal section production casing.

參考文獻/References:

[1] 梁興,朱炬輝,石孝志,等.縫內填砂暫堵分段體積壓裂技術在頁巖氣水平井中的應用[J]. 天然氣工業,2017,37(1):82-89.
[2] 楊毅,劉俊辰,曾波,等.頁巖氣井套變段體積壓裂技術應用及優選[J]. 石油機械,2017,45(12):82-87.
[3] 余夫,史偉.頁巖氣井套管變形失效原因分析[J]. 石油管材與儀器,2018,4(3):35-38.
[4] 李凡華,董凱,付盼,等. 頁巖氣水平井大型體積壓裂套損預測和控制方法[J]. 鉆井工程,39(4):69-75.
[5] 余道智.深層頁巖氣鉆井關鍵技術難點及對策研究[J]. 能源化工,40(1):69-73.
[6] 陳朝偉,石林,項德貴.長寧—威遠頁巖氣示范區套管變形機理及對策[J]. 天然氣工業,2016,36(11):70-75.
[7] 劉奎,高德利,王宴濱,等.局部載荷對頁巖氣井套管變形的影響[J]. 天然氣工業,2016,36(11):70-75.
[8] 喬磊,田中蘭,曾波,等.頁巖氣水平井多因素耦合套變分析[J]. 斷塊油氣田,2019,26(1):107-110.
[9] 郭雪利,李軍,柳貢慧,等.溫-壓作用下水泥環缺陷對套管應力的影響[J]. 石油機械,2018,46(4):112-118.
[10] 席巖,柳貢慧,李軍,等.頁巖氣井體積壓裂井筒溫度計算及套管強度變化分析[J]. 斷塊油氣田,2017,24(4):561-564.
[11] 董曉明,張忠鏵,羅蒙. 頁巖氣開發用高強高韌套管設計及適用性研究[J]. 石油管材與儀器,2017,3(1):47-51.
[12] 王春芳.低合金馬氏體鋼強韌性組織控制單元的研究[D]. 北京 :鋼鐵研究總院,2008.
[13] 沈俊昶,羅志俊,楊才福,等. 低合金鋼板條組織中影響低溫韌性的“有效晶粒尺寸”[J]. 鋼鐵研究學報,2014, 26(7):70-76.

相似文獻/References:

[1]董曉明,張忠鏵,羅蒙.頁巖氣開發用高強高韌套管設計及適用性研究[J].石油管材與儀器,2017,3(01):47.[doi:10.19459/j.cnki.61-1500/te.2017.01.011]
 DONG Xiaoming,ZHANG Zhonghua,LUO Meng.Design and Applicability Research of High Strength and Toughness Casing for Shale Gas Service[J].Petroleum Tubular Goods & Instruments,2017,3(04):47.[doi:10.19459/j.cnki.61-1500/te.2017.01.011]
[2]陳建波.連續油管分簇射孔技術發展現狀[J].石油管材與儀器,2017,3(03):7.[doi:10.19459/j.cnki.61-1500/te.2017.03.002]
 CHEN Jianbo.Current Situation of Coiled-tubing-conveyed Cluster Perforating Technology[J].Petroleum Tubular Goods & Instruments,2017,3(04):7.[doi:10.19459/j.cnki.61-1500/te.2017.03.002]
[3]余夫,史偉.頁巖氣井套管變形失效原因分析[J].石油管材與儀器,2018,4(03):35.[doi:10.19459/j.cnki.61-1500/te.2018.03.009]
 YU Fu,SHI Wei.Casing Deformation Failure Cause Analysis in Shale Gas Well[J].Petroleum Tubular Goods & Instruments,2018,4(04):35.[doi:10.19459/j.cnki.61-1500/te.2018.03.009]
[4]馬涌貴,朱坤,胡友良.MIT結合RBT測井資料在H油田套損評價方面的應用[J].石油管材與儀器,2018,4(05):11.[doi:10.19459/j.cnki.61-1500/te.2018.05.004]
 MA Yonggui,ZHU Kun,HU Youliang.Application of MIT and RBT Logging Data for Casing Damage Evaluation in H Oilfield[J].Petroleum Tubular Goods & Instruments,2018,4(04):11.[doi:10.19459/j.cnki.61-1500/te.2018.05.004]
[5]藍海峰,王開龍,杜衛強,等.存儲式套損檢測系統電池管理及主控短節開發[J].石油管材與儀器,2019,5(05):7.[doi:10.19459/j.cnki.61-1500/te.2019.05.002]
 LAN Haifeng,WANG Kailong,DU Weiqiang,et al.Development of Battery and Main Control Sub in Storage Type Casing Failure System[J].Petroleum Tubular Goods & Instruments,2019,5(04):7.[doi:10.19459/j.cnki.61-1500/te.2019.05.002]
[6]尹飛,韓禮紅,陳穎杰,等.頁巖氣井壓裂套管變形評價及水泥環性能優化[J].石油管材與儀器,2020,6(04):41.[doi:10.19459/j.cnki.61-1500/te.2020.04.007]
 YIN Fei,HAN Lihong,CHEN Yingjie,et al.Assessment of Casing Deformation and Optimization of Cement Sheath Performance Under Fracturing Shale Gas Wells[J].Petroleum Tubular Goods & Instruments,2020,6(04):41.[doi:10.19459/j.cnki.61-1500/te.2020.04.007]
[7]王宴濱,高德利,房軍.頁巖氣水平井壓裂過程水泥環力學特性評價研究[J].石油管材與儀器,2020,6(04):51.[doi:10.19459/j.cnki.61-1500/te.2020.04.009]
 WANG Yanbin,GAO Deli,FANG Jun.Assessment on the Cement Mechanical Properties of Shale Gas Horizontal Well in Fracturing Process[J].Petroleum Tubular Goods & Instruments,2020,6(04):51.[doi:10.19459/j.cnki.61-1500/te.2020.04.009]
[8]王建東,田濤,陳鷗,等.頁巖氣用生產套管螺紋連接選用和評價技術研究[J].石油管材與儀器,2020,6(04):63.[doi:10.19459/j.cnki.61-1500/te.2020.04.011]
 WANG Jiandong,TIAN Tao,CHENG Ou,et al.Selection and Evaluation Technology of Production Casing Threaded Connection for Shale Gas Wells[J].Petroleum Tubular Goods & Instruments,2020,6(04):63.[doi:10.19459/j.cnki.61-1500/te.2020.04.011]
[9]楊尚諭,韓禮紅,王建軍,等.頁巖氣井用套管承載特性試驗研究[J].石油管材與儀器,2020,6(04):69.[doi:10.19459/j.cnki.61-1500/te.2020.04.012]
 YANG Shangyu,HAN Lihong,WANG Jianjun,et al.Experimental Study on Casing Capacity for Shale Gas Well[J].Petroleum Tubular Goods & Instruments,2020,6(04):69.[doi:10.19459/j.cnki.61-1500/te.2020.04.012]
[10]張華禮,李玉飛,王漢.C-W區塊頁巖氣井大規模多級壓裂套管失效主控因素及防控措施分析[J].石油管材與儀器,2020,6(04):77.[doi:10.19459/j.cnki.61-1500/te.2020.04.014]
 ZHANG Huali,LI Yufei,WANG Han.The Main Control Factors and Responses for Casing Failure of Largescale Multistage Fracturing of Shale Gas Wells in C-W Block[J].Petroleum Tubular Goods & Instruments,2020,6(04):77.[doi:10.19459/j.cnki.61-1500/te.2020.04.014]
[11]李軍,丁士東,韓禮紅,等.頁巖氣多級壓裂井筒完整性失效機理及控制方法研究進展[J].石油管材與儀器,2020,6(04):10.[doi:10.19459/j.cnki.61-1500/te.2020.04.002]
 LI Jun,DING Shidong,HAN Lihong,et al.Research Progress on Failure Mechanism and Control Methods of Wellbore Integrity During Multistage Fracturing of Shale Gas[J].Petroleum Tubular Goods & Instruments,2020,6(04):10.[doi:10.19459/j.cnki.61-1500/te.2020.04.002]
[12]席巖,李軍,李方園,等.斷層滑移剪切套管變形內徑變化規律研究[J].石油管材與儀器,2020,6(04):38.[doi:10.19459/j.cnki.61-1500/te.2020.04.006]
 XI Yan,LI Jun,LI Fangyuan,et al.Variation of Inner Diameter After Casing Shear Deformation Induced by Fault Slippage[J].Petroleum Tubular Goods & Instruments,2020,6(04):38.[doi:10.19459/j.cnki.61-1500/te.2020.04.006]
[13]連威,李軍,柳貢慧,等.水力壓裂過程中頁巖強度折減對套管變形的影響分析[J].石油管材與儀器,2020,6(04):46.[doi:10.19459/j.cnki.61-1500/te.2020.04.008]
 LIAN Wei,LI Jun,LIU Gonghui,et al.Influence of Shale Strength Reduction on Casing Deformation During Hydraulic Fracturing[J].Petroleum Tubular Goods & Instruments,2020,6(04):46.[doi:10.19459/j.cnki.61-1500/te.2020.04.008]
[14]張慧,李軍,韓葛偉,等.瞬態力—熱耦合作用下套管應力影響因素分析[J].石油管材與儀器,2020,6(04):73.[doi:10.19459/j.cnki.61-1500/te.2020.04.013]
 ZHANG Hui,LI Jun,HAN Gewei,et al.Effects of Multifactor on Casing Stress Under Transient Thermalmechanical Coupling[J].Petroleum Tubular Goods & Instruments,2020,6(04):73.[doi:10.19459/j.cnki.61-1500/te.2020.04.013]
[15]黃永智,李軒,戴昆,等.頁巖氣生產套管損壞原因淺析與推薦解決方案[J].石油管材與儀器,2020,6(04):82.[doi:10.19459/j.cnki.61-1500/te.2020.04.015]
 HUANG Yongzhi,LI Xuan,DAI Kun,et al.Damage Causes and Solutions for Shale Gas Production Casing[J].Petroleum Tubular Goods & Instruments,2020,6(04):82.[doi:10.19459/j.cnki.61-1500/te.2020.04.015]

備注/Memo

備注/Memo:
第一作者簡介:張忠鏵,男,1969年生,教授級高級工程師,1998年畢業于東南大學金屬材料專業,獲博士學位,長期從事抗腐蝕油井管產品的開發研究工作。E-mail: [email protected]
更新日期/Last Update: 2020-08-25
湖北新11选5开奖公告